Wood is one of the first materials that was naturally and abundantly available to mankind. Therefore, the date of its use goes back a long time. Even though man started his life as a cave dweller, he used wood before other materials.
It has been proven for centuries that burning the surface of wood in fire makes it more resistant for outdoor use. In the production process of thermowood or thermo-heated wood, it is the same natural wood whose cell structure has been changed due to the production process of thermowood.
Heat-treated or heat-modified wood, which is waterproof, is known as Termwood.
✔️ Selection of special wood
In the production process of thermowood, thermo paint is used to protect and care for the freshness of thermo wood.
These colors (also called thermo resin), which are produced in Canada and Germany and are very popular in the Iranian market, are anti-UV and waterproof and increase the longevity of the product against the sun and rain.
See Thermowood colors...
Thermo wood is mainly produced from licensed forests in Europe and mostly in Finland, which is protected against the penetration of fungi, mold and termites by the thermo thermal mechanism without the use of chemicals and only by relying on heat, and is more durable than ordinary wood. It is much more. Also, this added heat in the Thermowood production process changes and transforms the uniform color of the product and makes the product more beautiful.
✔️ Drying wood
In the heating operation, water, steam, and high temperature are used. Compounds that evaporate from wood are corrosive.
The heating equipment is made of stainless steel, and in addition, for the high temperature, a special standard is required for the blower, radiator, and safety devices. To produce the heat needed in the thermowood production process, hot oil heating systems can be used, which work with oil or gas biofuels.
Other heating methods such as direct electric heating can also be used. In addition, the equipment used must have a steam generator to produce the steam required for this process. Gases evaporated from wood during the thermowood production process are managed by explosion and ignition.
✔️ Heating wood
In the continuation of the thermowood production process, the heating operation is carried out in a closed environment, in which the closed temperature increases from 185 to 215 degrees Celsius.
This phase starts immediately after the drying phase at high temperature. During the drying and heating stage, steam is used as a protection to prevent the wood from burning and also affects the chemical changes made in the wood.
When the wood is dried at a very high temperature, in the second stage of the thermowood production process, the oven temperature increases to about 180-215 degrees Celsius, depending on the standard type. After the temperature reaches this stage until the intended final use, the thermo wood is kept stable at this temperature for two or three hours, during which the presence of water vapor avoids burning.
✔️ Humidity and drying
In the last stages of the thermowood production process, water is regularly sprayed on the wood to reduce its temperature. When the temperature of thermo wood reaches about 80 to 90 degrees Celsius, it is moistened again to reach the appropriate humidity. The result of this work is the production of thermowood with 4-7% moisture. Basically, all the harmful bacteria inside the wood and the substances that change the shape of the wood are destroyed. In this 36-hour process, the wood is completely transformed and a completely new type of wood is created. Wood is aerated 2 to 3 hours after the heating operation, and after the heating operation, the wood is cooled while being carefully handled. Of course, great care is required because the extreme temperature difference between the wood chamber and the outside air can cause it to crack and break. In addition, during the production process of thermowood, the wood must be re-moisturized so that it has a suitable moisture for use. The final moisture level of wood has a significant effect on its functional properties because it is difficult to work with very dry wood. Besides, it is also effective in the price of thermowood. After aeration, the final humidity of the wood should be 5 to 7%, depending on the heating temperature and the type of wood, the aeration phase can last 5 to 15 hours.
✔️ Cutting in standard dimensions
At the end of the thermowood production process, if the heat treatment has been done correctly and the internal stresses have been released, the thermowood will not change shape after cutting. Because Thermowood does not contain resin, the required cutting force is reduced and the lifespan of the cutting equipment increases significantly. Even in filled wood, thermo wood cutting knot is different from normal wood cutting.
The only problem when cutting thermowood wood is wood dust. Because Termwood is very low in water, its sawdust is very fine and easily spread in the environment. For this reason, proper equipment is needed to remove sawdust from thermowood. The facilities used must be well sealed and effective enough because the high pitch of the cutting blade may cause the edges of the thermowood to fill up.